PROPERTY GENERAL | TEST | CONDITION | SI UNITS |
Specific Gravity | ASTM D 792 | 230C | 1.55 |
Specific Volume | 230C | 0.645 Cm3/g | |
Water Obsorption | ASTM D 570 | 230C | +0.03% |
Rockwell Hardness | ASTM D 785 | 230C | 119 |
MECHANICAL | |||
Izod Impact | ASTM D 256 | 230C | min. 80 j/m o.n. |
Tensile strength | ASTM D 638 | 230C | 55 N/mm2 |
Tensile Modulus | ASTM D 638 | 230C | 2500 N/mm2 |
Flexural Strength | ASTM D 790 | 230C | 104 N/mm2 |
Flexural Modulus | ASTM D 790 | 230C | 2860 N/mm2 |
Compressive strength | ASTM D 695 | 230C | 70 N/mm2 |
Compressive Modulus | ASTM D 695 | 230C | 1350 N/mm2 |
THERMAL | |||
Coefficient of Thermal Expansion | ASTM D 696 | 6.3 x 10-5m/m/k | |
Thermal Conductivity | ASTM C 177 | 0.14 Wm/k/m2 | |
Heat Distortion Tempreture | ASTM D 638 | 100C | |
Hit Capacity | DSC | 230C | 0.90 j/gk |
1000C | 1.10 j/gk. | ||
FLAMMABILITY | |||
Flammability Rating | UL94 | 0.062 in/0.157 cm | V-0 |
Flame Speed | ASTM E84 | 15 | |
Smoke developed | ASTM E84 | 70-125 | |
Limiting Oxygen Index | ASTM D 2863 | 60 | |
ELECTRICAL | |||
Dielectric Strength | ASTM D 147 | 4.92000 V/cm | |
Dielectric Constant | ASTM D 150 | 60 Hz, -10c | 3.7 |
Power Factor | ASTM D 150 | 1000 Hz | 0.007 % |
Volume Resistivity | ASTM D 257 | 230c | 3.4×1015ohm/cm |